Fig. 21
Quickly pour the loose welding material powder into
the CADWELD EXOLON mold.
NOTE: Welding material is an exothermic
mixture and reacts to produce hot molten
material with temperatures in excess of 2500
degrees Fahrenheit (1400 degrees Celsius) and
a localized release of smoke. Avoid direct eye
contact with “flash” of light from ignition of
starting material. Avoid inhalation of smoke/
fumes.
Fig. 22
Place the graphite CADWELD EXOLON cover onto the
mold, with the larger side facing down.
Fig. 23
Next, take an igniter pin and place it halfway into the
small hole on the side of the mold, with the loop side
facing into the hole. Spread the wire leads.