VI–6
PLASTIC BODY PARTS
2. Weld the damaged area.
For repair of a cracked area, melt the crack together with a heat gun and a melting attachment.
For repair of a hole, degrease the area on both sides of the bumper and apply aluminium tape on the
reverse side of the damage area.
3. Melt the polypropylene welding rod with a heat gun and deposit it the cracked area.
Note
Heat the shaded area to melt it.
Take care not to overlay melt welding rod. If the part is welded with the welding rod melted like jelly, the
welding strength will be reduced.
Hold the heat gun 10—20 mm {0.39—0.79 in} from the part being welded.
Do not move the welding rod until the welded parts cool.
ZUA9818B003
ZUA9818B005
ZUA9818B004