25
W 200
GB
Problem Cause Remedy
Coating material
drips from the
nozzle
•
Coating material assembly
at air cap, nozzle or needle
•
Nozzle loose
•
Nozzle seal worn
•
Nozzle worn
➞ Clean
➞ Union nut tighten
➞ Change
➞ Change
Atomisation too
coarse
•
Material volume too large
•
Material volume adjusting
screw turned too far to the
right (+)
•
Nozzle contaminated
•
Viscosity of coating material
too high
•
Too little pressure build-up
in container
•
Air lter heavily soiled
➞ Turn material volume
adjusting screw to the
left(-)
➞ Clean
➞ Dilute further
➞ Tighten container
➞ Change
Spray jet pulsates
•
Coating material in
container running out
•
Nozzle seal worn
•
Air lter heavily soiled
➞ Rell
➞ Replace
➞ Change
Coating material
causes "paint tears"
•
Too much coating material
applied
•
Viscosity of coating material
too low
➞ Turn material volume
adjusting screw to the left(-)
Too much fog of
coating material
(Overspray)
•
Distance to the object too
large
•
Too much coating material
applied
➞ Reduce distance
➞ Turn material volume
adjusting screw to the left (-)
Paint in the
ventilating hose
•
Diaphragm soiled
•
Diaphragm defective
➞ Clean the diaphragm
➞ Replace the diaphragm
18. Technical Data
Technical Data
Max. viscosity: 170 DIN-s
Power source: 230 V, ~ 50 Hz
Power consumption: 460 W
Atomizing output: 130 W
Max. ow rate: 150 ml/min
Double insulation: