16
4.3.3 Weekly
After re-charging, carry out a visual inspection for dirt and physical damage.
If the battery is charged regularly according to the IU characteristic, carry out a
compensation charge.
4.3.4 Monthly
Towards the end of the charging process measure and record the voltages of all
the cells with the charger switched on.
After charging measure and record the electrolyte density and the electrolyte
temperature in all the cells.
Compare the results with the previous ones.
Z If you find significant differences compared with the previous measurements or
differences between the cells, contact the manufacturer's customer service
department.
4.3.5 Annually
Measure the insulation resistance of the truck in accordance with EN 1175-1.
Measure the insulation resistance of the battery in accordance with DIN EN 1987-1.
Z In accordance with DIN EN 50272-3 the battery insulation resistance should not be
less than 50 Ω per volt of rated voltage.

Table of Contents

Questions and Answers:

Question and Answer IconNeed help?

Do you have a question about the Jungheinrich ERC 214z and is the answer not in the manual?

Jungheinrich ERC 214z Specifications

General IconGeneral
BrandJungheinrich
ModelERC 214z
CategoryForklifts
LanguageEnglish

Related product manuals