COPPERAISI 316CONCENTRATION
mg/l or ppm
WATER CONTAINING
Alcanity (HCNO
3)
Sulfate (SO
4
2-
)
HCO
3 / SO4
2-
Electrical conductivity
pH
Ammonium (NH
3)
Chloroides(Cl
-
)
Free chlorine (Cl2)
Hydrogen sulfide (H
2S)
Free (aggressive) Carbon Dioxide (CO
2)
Total hardness (ºdH)
Nitrate (NO3)
Iron (Fe)
Aluminum (Al)
Manganese (Mn)
0
+
0
+
-
-
+
-
0
+
0
0
0
+
0
+
0
-
+
0
+
0
-
+
-
+
0
-
+
0
+
0
+
0
+
0
+
+
+
+
+
+
0
+
+
+
+
+
0
0/+
+
+
+
+
+
+
0
+
+
0/+
+
+
+
+
+
+
+
+
+
+
+
+
+
+
<70
70-300
>300
<70
70-300
>300
>1.0
<1.0
<10 mS/cm
10-500 mS/cm
>500 mS/cm
<6.0
6.0-7.5
7.5-9.0
>9.0
<2
2-20
>20
<50
>50
<1
1-5
>5
<0.05
>0.05
<5
5-20
>20
4.0-8.5
<100
>100
<0.2
>0.2
<0.1
>0.1
<0.2
>0.2
GUIDE TO MEASURE A ANALYSIS OF THE WATER IN THE CIRCUIT.
The resistance guide below is an attempt of give a picture of the corrosion resistance of the stainless steel of the
type AISI 316 and pure copper in the water, to a number of important chemical factors. The actual corrosion is however
a very complex process influenced by many factors in combination. This table is therefore a considerable simplification
and should not be overvalued.
Explanations:
+ Good resistance under normal conditions
0 Corrosion problems can occur especially when the factors are valued as 0
- Use is not recommended
3.3.- CORROSION RESISTANCE OF COPPER AND STAINLESS STEEL OF PLATES EXCHANGER
(WATER EXCHANGER)