3.3 Material of the facility built
Facility
Components
Weight(g)
Weight
percentage
Selective treatment for materials
and components
Details
1.
62
2.8%
Fe recycling
2
810
36.0%
Fe recycling
3
51
2.3%
Containing brominated flame
retardants
4
8.0
0.4%
Containing brominated flame
retardants
5
10
0.4%
The surface of PCB is greater
than 10 square centimeters
6
478
21.2%
The surface of PCB is greater
than 10 square centimeters
7
721
32.0%
Fe recycling
8
N/A
N/A
N/A
9
6.5
0.3%
Containing brominated flame
retardants
10
N/A
N/A
N/A
11
87
3.9%
The surface of PCB is greater
than 10 square centimeters
12
15.4
0.7%
Containing brominated flame
retardants
13
2.0
0.1%
Containing brominated flame
retardants
4. Revised record