Energy Settings 
 
Arc Welding 
 
The  following  settings  may  be  used  as  a  guide.  The  correct 
setting for a particular metal combination and wire gauge will 
produce  a  spherical  bead.  A  flattened bead  indicates  that  the 
energy setting is too high. 
 
Wire Diameter (mm) 
 
Switch at “LOW”  0.1    Switch at “HIGH”  0.3 
        0.15          0.5 
        0.2            0.7 
        0.25          0.8 
 
 
 
Electrodes 
To replace or adjust carbon electrode, first turn the welder on 
its side and slacken screw on base of argon shield, which may 
be then pulled off.  This reveals grub screw which holds  car-
bon electrode in place. 
 
- 7 -