How to fix pore creation with ASKAYNAK MASTERMIG 420W?
- SSamuel KingAug 17, 2025
Pore creation during welding with your ASKAYNAK Welding System can stem from several factors: * Insufficient gas shielding: Increase gas flow, clean the nozzle, prevent gas hose leakages, and block airflows. * Dirty gas or unsuitable gas flow: Use quality welding gas and adjust the flow rate. * Dirty welding wire: Ensure you're using clean, dry welding wire. * Dirty workpiece: Remove oil, grease, rust, paint, and dirt from the workpiece surface. * High voltage: Decrease the voltage value. * Excessive distance between nozzle and workpiece: Shorten the free wire length.