28
Attention:
Flow is proportion of filament , we suggest to use 100
Increasing flow & decrease diameter has the similar
effect.
Model surface gets many bumps when flow is too
big;model frame gets flimsy if flow is too small.
Attention: A8 use 1.75mm filament
We suggest not to change
it , A8 default 0.4mm
We suggest not to change it ,
or use the date in the picture
We suggest 0.2mm to avoid initial layer tilt,0.3mm
is more easy to seperate from the platform.
Initial layer line proportion
“0” means using default speed
Min printing time for each layer. When the time is
less than 10 , it prints slower. It’s better to
decrease time when printing thin and long models.
We suggest not choose this when printing ABS.