English ⋅ Nautilus
®
CC plus ⋅ Nautilus
®
T
35
86105 BA-en/00
Table of holding times / further heating times
* Specified in seconds.
** During the holding time the selected casting temperature is maintained.
For manual casting*
Group Alloy Program
with pyrometer:
Holding times**
without pyrometer:
add. heating times
Au Bio PlatinLloyd
®
118 15 14 to 17
Bio PontoStar
®
154 15 15 to 18
Bio PontoStar
®
XL 155 15 17 to 22
InLloyd
®
100 115 16 17 to 20
PlatinLloyd KF 111 16 10 to 13
PlatinLloyd M 113 19 10 to 13
PlatinLloyd 100 114 19 10 to 13
PontoLloyd
®
G 158 13 22 to 25
PontoLloyd
®
L 157 11 12 to 15
PontoLloyd
®
P 156 12 18 to 22
Pontonorm 119 17 12 to 15
PontoRex
®
G 117 17 12 to 15
PontoStar
®
G 151 13 17 to 20
PontoStar
®
H 152 13 17 to 20
Au AuroLloyd
®
KF 121 15 17 to 20
AuroLloyd
®
M 123 18 17 to 20
BegoCer
®
G 162 10 12 to 18
BegoLloyd
®
LFC 126 17 17 to 20
BegoLloyd
®
M 125 19 17 to 20
BegoStar
®
163 12 22 to 25
Midigold
®
128 19 17 to 20
Pd BegoPal
®
171 10 13 to 16
BegoPal
®
S 172 10 13 to 16
BegoPal
®
300 173 10 13 to 16
BegoPal
®
164 10 13 to 16
BegoPal
®
S 165 10 13 to 16
BegoPal
®
300 166 10 13 to 16
Ag Silver-gold-palladium 131 approx. 14 17 to 20
BegoStar
®
LFC 142 14 17 to 20
ECO d’OR 132 14 17 to 20
Eco BegoStar
®
ECO 174 10 3 to 7
BegoStar
®
ECO 167 10 3 to 7
NiCr Wirocer plus 197 0 6 to 12
Wiron
®
99 191 0 7 to 10
Wiron
®
light 199 0 3 to 7
CoCr Wirobond
®
C 192 0 7 to 10
Wirobond
®
LFC 193 0 4 to 8
Wirobond
®
SG 196 0 2 to 4
Wirobond
®
280 195 0 2 to 4
Wironit
®
184
0 7 to 10
Wironit
®
extra-hard 185 0 6 to 9
Wironit
®
LA 186 0 6 to 8
WIRONIUM
®
181 0 2 to 4
WIRONIUM
®
extra-hard 182 0 6 to 8
WIRONIUM
®
plus 183 0 6 to 8