Mimaki Europe B V
Industrial Products
LED UV INK
• Solvent resistance & Dipping test
• When printing on less adhesive media, UV ink tends to peel off by the
penetration of water or solvent from the print edge.
LH-100 LUS-150
Water
× ○
Hot water (60℃)
× △
*1
Ethanol (100%)
○ ××
*2
Xylene (100%)
△ ××
*2
Evaluation standards :
○:Attached
△: Peels off partly
×:Takes some time to peel off
××:Peels off immediately after dipping(It takes 3 minutes to peel off when dipping in ethanol and xylene)
*1: Air bubbles get in/ 2: Ink film is attacked
40