Evaluation of findings and further measures
The findings in the start phase of oxidation discoloration and heat discoloration are similar. A thorough inves-
tigation and compliance with the above evaluation criteria allow an unambiguous evaluation. To avoid unnec-
essary disassembly work, it is recommended that another inspection be carried out after further operation of
the engine.
76 | Cylinder Liner | MS150060/04E 2016-02