Step Key (or instruction) Display/Printout
6. Prepare the sample: not necessary
for dispersion adhesive
7. Open the sample chamber k key
Position a new sample pan
8. Tare the sample pan
Tare soft key
9. Apply approx. 1.5 g of
dispersion adhesive uniformly
to the sample pan
Close the sample chamber k key
10. Start the drying program
Start soft key
After 2 seconds’ delay --------------------
the header for moisture 14.07.1999 17:10
analysis is printed
Mod. MA100C
Ser. no. 90805355
Ver. no. 01-38-07
ID
--------------------
Prg 5 DISP ADHESIVE
Heating PHASES
Temp.1 140
C
Time1 5.0 min
Temp.2 140
C
Time2 0.0 min
Fin. temp. 140
C
Stdby temp. OFF
Start W/STABIL.
End AUTOMATIC
IniWt + 1.502 g
--------------------
The current moisture loss
displayed afterwards
49
Info ID Stat. Mode Prog.
P5 140/140/140 C Auto.
WEIGH-IN: Load sample pan
+ 0000 g
Info ID Stat. Mode Prog.
P5 140/140/140 C Auto.
WEIGH-IN: Start analysis
+ 1502 g
Start
ID Stat. Para. Prog.
P5 140/140/140 C Auto.
ANALY.BEGIN: Start delay 2sec
+ 1502 g
Abbr.
S
Info ID Stat. Mode Prog.
P5 140/140/140 C Auto.
ANALYSIS: 27 C 0.3min ----mg/24s
+ 006 %L