EasyManua.ls Logo

CIGWELD 200AC - Page 55

CIGWELD 200AC
70 pages
Print Icon
To Next Page IconTo Next Page
To Next Page IconTo Next Page
To Previous Page IconTo Previous Page
To Previous Page IconTo Previous Page
Loading...
WELDSKILL 200 AC/DC INVERTER
Manual 0-5207 4-17 BASIC WELDING GUIDE
7 Dirty weld pool A Electrode contaminated
by contact with work
piece or filler rod mate-
rial.
A Clean the electrode by grinding off the
contaminates.
B Work piece surface has
foreign material on it.
B Clean surface.
C Gas contaminated with
air.
C Check gas lines for cuts and loose fitting
or change gas cylinder.
8 Poor weld finish Inadequate shielding
gas.
Increase gas flow or check gas line for
gas flow problems.
9 Arc start is not smooth. A Tungsten electrode is
too large for the weld-
ing current.
A Select the right size tungsten electrode.
Refer to Table 4-3 CIGWELD Tungsten
Electrode Selection Chart.
B The wrong electrode
is being used for the
welding job.
B Select the right tungsten electrode type.
Refer to Table 4-5 CIGWELD Tungsten
Electrode Selection Chart.
C Gas flow rate is too
high.
C Select the right rate for the welding job.
Refer to Table 4-7.
D Incorrect shielding gas
is being used.
D Select the right shielding gas.
E Poor work clamp con-
nection to work piece.
E Improve connection to work piece.
10 Arc flutters during TIG
welding.
Tungsten electrode is
too large for the weld-
ing current.
Select the right size tungsten electrode.
Refer to Table 4-3 CIGWELD Tungsten
Electrode Selection Chart.

Related product manuals