4.
Create the denture resin.
A
Insert into the lidded container all the measured heated polymerizing resin liquid.
B
Insert 80% of the measured heated polymerizing resin powder so it ts below the liquid surface.
C
Insert the remaining 20% of the powder to cover the liquid surface.
D
Close the lid and mix the components together.
E
Wait 2 to 3 minutes until the mixture becomes porridge-like. If the room temperature is low, you may have to wait
a little longer.
F
Fix the FX onto the protrusion in the silicone stand.
Align the hole drilled in step 1. with the protrusion on the silicone stand.
Supplemental
Applying vegetable oil to the protrusion on the silicone stand makes it easier to remove the resin after polymerization.