O
Perform the pre-polymerization.
Gradually increase the water temperature to 65°C (149°F), and then perform pressurized and heated polymerization at 65
°C (149°F) for 90 to 120 minutes.
Important
The pre-polymerization time is merely a guideline. If cracks or air bubbles remain in the heated polymerizing resin being
used, increase this time until there are no cracks or air bubbles.
P
Perform the polymerization.
Perform pressurized and heated polymerization at 80°C (176°F) for 40 minutes.
Important
Heated polymerizing resin polymerizes at high temperatures. Handle it carefully after polymerization to avoid burns.
Q
Remove the FX from the silicone stand, and then leave the FX at room temperature for approximately 30 minutes.
R
Cool the FX for approximately 15 minutes with cold water.
5.
Mill the denture resin.
A
Remove the adapter cap.
Use a torque screwdriver to loosen the adapter's cap screws by turning them approximately four times each, and then re-
move the adapter cap.
B
Attach the adapter base to the FX.
Align the edge of the adapter (A) with the edge of the FX (B).
C
Attach the adapter cap.
Usage Method