settings are not configured properly, the printer may extruder more plastic than
the software expects. This over-extrusion will result in excess plastic that can ruin
the outer dimensions of your part. To resolve this issue, there are only a few
settings you need to verify in Anet3D control panel. Please see the Not Extruding
Enough Plastic section for a more detailed description. While those instructions
are for under-extrusion, you will adjust the same settings for over-extrusion, just
in the opposite direction. For example, if increasing the extrusion speed helps
with under-extrusion, then you should decrease the
extrusion speed for over-extrusion issues.