54
Poor weld properties
(severe spattering)
Cause: Incorrect electrode polarity
Remedy: Reverse electrode polarity (refer to manufacturer's instructions)
Cause: Poor grounding (earthing) connection
Remedy: Fasten earthing clamps directly to workpiece
Cause: Setup parameters not ideal for selected welding process
Remedy: Select the optimal settings in the Setup menu for the selected welding pro-
cess
Tungsten electrode melting
Tungsten inclusions in base metal during the ignition phase
Cause: Incorrect tungsten electrode polarity
Remedy: Connect the TIG welding torch to the (-) current socket
Cause: Incorrect (or no) shielding gas
Remedy: Use inert shielding gas (argon)
VRD does not light up even though no welding process is taking place
Cause: VRD option not present
or internal device fault
Remedy: Contact after-sales service