Page 28 of 28
4
High
Temperature
Material
Disco
Purge
Off
High temperature
material preheat
temperature minus
25C.
Temperature can vary
depending on material
type and grade. Special
exception to ABS where
the removal
temperature is the
same as the preheat
temperature.
High temperature
material extrusion
temperature minus
~10C.
Temperature can vary
depending on material
type and grade.
High temperature
minimum extrusion
temperature specified
in manufacturer's
MSDS document.
Cross reference materials
extrusion temperatures when
purging dissimilar materials. If
the minimum extrusion
temperature for the high
temperature material is higher
than the maximum extrusion
temperature of the low
temperature material then you
will risk burning the low
temperature material and
clogging your extruder. If there is
no overlap in material processing
temperatures, you may require
an intermediary purge material.
5
Colour 1
Short
Purge
On
Material Dependent.
Material Dependent.
Material Dependent.
Run extruder in manual mode
until purged of previous colour
and fully transitioned to the new
colour. Colour can also be
switched at any time during
regular extrusion.
6
Wet Plastic
Short
Purge
On
Material Dependent.
Material Dependent.
Material Dependent.
Run extruder in manual mode
until purged. Plastic may be wet
if you notice necking or bubbles
(or pockets) in extrusion. You
can leave nozzle on for wet to
dry plastic conditions.

Other manuals for ReDeTec ProtoCycler