Manual 0-4989 4T-9 OPERATION
Slag Buildup
Slag generated by gouging on materials such as carbon and stainless steels, nickels, and alloyed steels, can be
removed easily in most cases. Slag does not obstruct the gouging process if it accumulates to the side of the
gouge path. However, slag build - up can cause inconsistencies and irregular metal removal if large amounts of
material build up in front of the arc. The build - up is most often a result of improper travel speed, lead angle,
or standoff height.