26
MA201435_13.1 [Original Instructions] 6/25/2012
Trouble Shooting when using Thermosetting Resins
Thermosetting resins include Phenolic, Diallyl Phthalate, EpoMet™, and KonductoMet™.
Mold appears grainy
and unfused.
Curing temperature too low.
Increase cure temperature.
Insufficient molding
pressure.
Increase molding pressure.
Increase heat time.
Increase molding pressure.
Sample corners too sharp.
Decrease sample size.
Round sample edges.
Store resin in a dry area.
Keep resin containers closed.
Dry resins at low
temperatures.
Clean and dry specimens
thoroughly.