5.3.3 Further welding parameters
NAVIGATION
B
A
A
A
A
A
A
B
B
B
B
ENTER EXIT
3 s
l
0
Figure 5-15
Display
Setting/selection
Dynamic correction
Increase value > harder arc
Decrease value > softer arc
Gas pre-flow time
Gas post-flow time
Correct wire burn-back
If too high a value is set, a large ball will form at the tip of the wire electrode (bad re-
ignition) or the wire electrode sticks to the contact tip. If too low a value is set, the wire
electrode sticks to the weld pool.
Increase value > increase wire burn-back
Decrease value > decrease wire burn-back
Wire creep