Note:
A vertical line sometimes appears at the splice point when MM bers or dissimilar
bers (dierent diameters) are spliced. We call it as “Splicing line”. This does not
aect splice quality (such as splice loss and tensile strength).
Fat
Fiber stung too
much
Decrease [Overlap] and
Perform [Arc Calibration].
Thin
Arc power not
adequate
Perform [Arc Calibration].
Some arc
parameters not
adequate
Adjust [Pre-fuse Power],
[Pre-fuse Time] or
[Overlap].
Splicing line
Some arc
parameters not
adequate
Adjust [Pre-fuse Power],
[Pre-fuse Time] or
[Overlap]