Turn the knob to find the required IPM
Select 2T / 4T / Spot
If you select spot mode
Please adjust the spot time
Select inductance level
/
Select Bum-back time
You can also choose to use the default Settings
NOTICE:
Always weld clean, dry and well-prepared
material.
Hold gun at a 45° angle to the workpiece with
nozzle about 1/2” from the surface.
Move the gun smoothly and steadily as you weld.
On thin gauge material, move quickly and only
weld 1/4” stitch-welds at a time to avoid
melt-through.
Avoid welding in very drafty areas. A weak, pitted
and porous weld will result due to drafts blowing
away the
Keep wire and liner clean. Do not use rusty wire.
Sharp bends or kinks in the welding cable should be avoided
ONLY use MIG solid welding wire.
MIG Welding parameters tablefor reference only