6 CONTROL PANEL
0463 479 001
- 32 -
© ESAB AB 2017
Preflow The time the
shielding gas stays on
before the welding arc is
started
Smart MIG
Postflow The time the
shielding gas stays on after
the welding arc is stopped
Cancel
Seconds
Saving welding programs for
a specific application when in
the Memory Mode
Settings on user manual
menu
Burnback Adjusting the time
when the voltage stays on
after the wire feed is stopped
to keep the wire from freezing
in the weld puddle
Spool Gun Stick
2T, Trigger On/OFF Lift-TIG
4T, Trigger Hold/Lock User Manual on main menu
Amps
Plate thickness at sMIG
mode
Arc force On stick
welding-increasing amps
when the arc length is
shortened to reduce or
eliminate the freezing of the
stick electrode in the weld
puddle
Trim bar Changing the weld
bead profile from flat to convex
or flat to concave
Downslope Sloping the
current down over a period
of time at the end of the
weld cycle
Bead profile, concave
Hot start The increase of
amps when striking the
electrode to reduce sticking
Bead profile, convex