• Parts made of High Temperature RGD525 have a thermal resistance:
• Heat Deflection Temperature (HDT) of 65 °C (149 °F)
• With post thermal treatment , you obtain higher thermal resistance:
• Up to 80 °C (176 °F)
• To achieve the expected HDT, post thermal treatment is required based
on a procedure.
• For additional information refer to the application note
Post Process – Post Thermal Treatment