Model 4140
4-3
COMPACTING THE SPECIMEN
The following is a checklist for compacting an asphalt specimen
with the Model 4140. Each step is discussed in detail in the
following text.
Set up the gyratory compactor.
Prepare the specimen.
Clean the turntable and loading head with a degreasing cleaner.
If compacting at angles less than 0.7°, then convert the unit for
small angle compaction (see page 3-18) and before each
compaction cycle, apply a light lubricant such as Slick 50 One
Lube to the turntable.
Compact the asphalt specimen.
Remove the mold containing the compacted specimen from the
compactor.
Extrude the asphalt specimen from the mold.
SETTING UP
The Model 4140 requires some set up before compacting a
specimen (see page 2-9). Check the number of gyrations and
pressure (see page 2-10). If the user wants to automatically output
gyration versus height data, connect the control unit to the computer
or printer and turn on the Auto Output option (see page 2-12). To
print the pressure-versus-height data, turn on the Pressure Printout
feature (see page 2-17).
4. MAKING A SPECIMEN

Questions and Answers:

Question and Answer IconNeed help?

Do you have a question about the Troxler 4140 and is the answer not in the manual?

Troxler 4140 Specifications

General IconGeneral
BrandTroxler
Model4140
CategoryLaboratory Equipment
LanguageEnglish

Related product manuals