Apply two (2) thin layers of glue to the center of the plate. Select the checkmark to continue.4.
NOTE: For more information, refer to the section titled Applying Cube Glue.
NOTE: For small print file sizes, use a light coating of glue. For larger parts, a slightly
thicker coating of glue is recommended. When the printer begins to print, the glue
surface should be mostly dry. The temperature from the print material will melt the
surface of the glue increasing its adhesion.
NOTE: Ensure that the area where glue is applied is larger than the base of your
creation.
NOTE: The estimated time to completion is noted at the bottom of the screen.
NOTE: The estimated time to completion is noted at the bottom of the screen.
NOTE: When printing with ABS material, the print chamber will need to build and
maintain a predetermined temperature. Ensure the top cover and the back panel have
been installed. The front door must be closed.
NOTE: When printing with PLA only or both PLA and ABS material, the print chamber
will not need to be preheated.
NOTE: The print jets required for the print job will begin to heat.
CAUTION: Do not touch the print jets until they have cooled to room temperature.