Zirlux FC2 Mill Maintenance
It is necessary to clean the mill and change the water before milling Zirlux FC2. If the zirconia is
contaminated with other materials, it will turn green when sintered. Cleaning after milling is recommended
because the zirconia acts as a thickening agent with the water.
Zirlux FC2 Scale Factor
See the manufacturers Instructions for Use provided with the Zirlux FC2 blocks for processing instructions.
Zirconia shrinks in the sintering oven. There are numbers on the side of the box that the blocks come in. You
must keep this box with the blocks. Do not mix blocks from di erent boxes. Each box can have a di erent
amount of shrinking. The Milling Center asks for the Scale Factor before a Zirlux FC2 is milled. The system
will increase the size of the restoration according to this number. This means you cannot test the  t of the
restoration before sintering.