Shini Group
Technology & Marketing Dept
Issued by department: Date: Language: Document Name: Revision: Page:
Shini/CSC-TM
2013-11 zh-cn Shini product repair manual.doc
1.0 24 (62)
Catalog:
template:Standard_CN.dot; filename: Shini product repair manual; Printdate: 8/1/2014 1:58:00 PM; savedate: 8/1/2014 1:58:00 PM
9.3.2 Regeneration temperature is set incorrectly
If the honeycomb material is silicone, the regeneration temperature is set to 150
℃; If honeycomb material is molecular sieve, regeneration temperature should be
set to 180℃.
Pic 9-3