Maintenance8752−1/A1
RT-flex58T-D
Winterthur Gas & Diesel Ltd.
4/ 5
4. Regrinding of sealing faces ’DF’
4.1 With regrinding device 94870
In order to achieve a clean and smooth sealing face the following regrinding pro-
cess is recommended. For deep notches > 0.1 mm choose emery cloth of medium
to coarse grade. Once the deep notches have been ground off, use a fine or ultra
fine emery cloth.
D
E
016.738/08
016.738/08
94870H
EC
94870F
GRAINED FACE
TIGHTENED
CONDITION
⇒ Place template 94870H on the back of emery cloth
’EC’ .
⇒ Trace inner contour using a pointed pencil or a ball
pen.
⇒ Cut out precisely the traced contour.
⇒ Shape the cut cloth in a manner to obtain a cone with
the grained face being turned inward.
⇒ Place the emery cloth in the cone of the grinding tool
94870F and fix it by means of its countersunk screw.
HP Fuel Pipe: Removing, Fitting and Regrinding