Koehring Spec 805 Data
PHYSICAL
PROPERTIES
TEST METHOD REQUIREMENT
A. A.P.I. Gravity ASTM D287 28 Min.
B. Flash Point ASTM D92 380× F Min.
C. Viscosity Index
100×F
210×F
ASTM D445
ASTM D445
200-220 SSU
46 SSU MIn.
D. Viscosity Index ASTM D2270 95 Min.
E. Pour Point ASTM D97 -25× F Max.
F. Oxidation Test to
2.0 Neut. No.
ASTM D943 2500 Hours Min.
G. Rust Test ASTM D665
Procedure A
Pass
H. Foam Test ASTM D892
Sequence I
Sequence II
Sequence III
Foam Tendency
25 ml Max.
50 ml Max.
25 ml Max.
Foam Stability
Nil
10 ml Max.
Nil
I. Demulsibility ASTM D1401 to
40-37-3 point
30 Min. Max.
J. Aniline Point ASTM D611 200-230× F
K. Pump Wear Dennison HFO or
Vickers M2905 (100
Hrs.@150× F)
Satisfactory
L. % Zn ASTM D1549 .07 Min.
M. Filterability Fluid shall show no additive loss when
filtered through 5.0 micron filter.
N. Cleanliness Fluid shall appear bright and clear and shall
be free of visible contaminates or sludge.