155
EN
Recognising
faulty wearing
parts
1. Insulating parts
– Burned-off outside edges, notches
2. Nozzle fittings
– Burned-off outside edges, notches
– Heavily covered in welding spatter
3. Spatter guard
– Burned-off outside edges, notches
4. Contact tips
– Worn-out (oval) wire entry and wire exit holes
– Heavily covered in welding spatter
– Fusion penetration on the tip of the contact tube
5. Gas nozzles
– Heavily covered in welding spatter
– Burned-off outside edges
– Notches