23
38. Photocuring options – Select the curing mode: Always on, during extrusion only, or layer-by-
layer. (The extrusion and layers -options require a Duet-TCB connection. Contact Brinter for
more information.)
39. UV post curing settings – Tick the box to enable post-curing after the printing process. The
same wavelength and intensity percent are used for post-curing as for curing during printing
if the Duet-TCB connection upgrade kit has not been installed.
40. Duration – Adjust the duration of the post-curing in seconds.
41. Curing manual – Click the link to open a separate document about the measured intensity
values (mW/cm
2
) for in situ curing with 365 nm, 405 nm, and 450 nm tool-integrated LEDs.
42. Save material – After configuring all the printing parameters for the material, click SAVE
MATERIAL.