Recognising
faulty wearing
parts
1.
Insulating parts
-
Burned-off outside edges, notches
2.
Nozzle fittings
-
Burned-off outside edges, notches
-
Heavily covered in welding spatter
3.
Spatter guard
-
Burned-off outside edges, notches
4.
Contact tips
-
Worn-out (oval) wire entry and wire exit holes
-
Heavily covered in welding spatter
-
Penetration on the tip of the contact tip
5.
Gas nozzles
-
Heavily covered in welding spatter
-
Burned-off outside edges
-
Notches
Replacing the