Finisher/Booklet Finisher
The Leading Edge of Paper Rolls Up (JAM607 / JAM609)
Cause:
A3 or larger paper with a thickness of Paper Weight 1 (cross-grain direction) or Paper Weight 2 (grain
direction) are delivered with a face-up curl (approximately 15 mm (0.6 inches)), resulting in the leading
edge of the paper riding up and rolling upward.
On the other hand, the leading edge of paper with a thickness of Paper Weight 0 may droop, resulting
in a steep contact angle with the output tray and the leading edge of paper rolling downward. Such a
face-down curl is prone to occur especially when delivering the paper face up.
If the face-up curl is severe (15 mm (0.6 inches) or more), the leading edge of the paper will ride up
and roll upward.
The leading edge of the paper curls downward
11. Post-Processing Option Troubleshooting