EasyManua.ls Logo

Cloos QINEO - Normal CW; Rapid Weld

Cloos QINEO
186 pages
Print Icon
To Next Page IconTo Next Page
To Next Page IconTo Next Page
To Previous Page IconTo Previous Page
To Previous Page IconTo Previous Page
Loading...
52
MAIN process
5.7.2 Normal CW
This is a MIG/MAG welding process without pulse but with synergy func-
tion. The welding current depends on the distance between torch and
workpiece. In connection with the QIROX robot application, arc seam track-
ing is possible to a limited extent. This welding process is suitable for sheet
thicknesses from 0.5 mm - 3.0 mm.
5.8 Rapid Weld
The Rapid Weld process generates a very concentrated arc during the weld-
ing process, which guarantees a very deep penetration.
The following characteristic curves are available as Rapid Weld variant:
• Normal, Fe, 92 % Ar, 8 % CO
2
, wire 1.0 mm
• Normal, Fe, 92 % Ar, 8 % CO
2
, wire 1.4 mm
• Normal, Fe, 82 % Ar, 18 % CO
2
, wire 0.8 mm
• Normal, Fe, 82 % Ar, 18 % CO
2
, wire 1.0 mm
• Normal, Fe, 82 % Ar, 18 % CO
2
, wire 1.2 mm
• Normal, Fe, 82 % Ar, 18 % CO
2
, wire 1.4 mm
• Normal, Fe, 82 % Ar, 18 % CO
2
, wire 1.6 mm
• Normal, Fe, 91 % Ar, 4 % O
2
, 5% CO
2
, wire 1.2 mm
• Normal, Fe, 91 % Ar, 4 % O
2
, 5% CO
2
, wire 1.4 mm
• Normal, Fe, 91 % Ar, 4 % O
2
, 5% CO
2
, wire 1.6 mm
To activate the Rapid Weld characteristic curve, you have to select one of
the above mentioned characteristic curves and the variant 1 M or Rapid
Weld at the PREMIUM operating module.
(Main/Synergy/Variant --> variant 1 M).
INFO!

Table of Contents

Related product manuals